Close
联系我们
信息反馈
在线订购

Economic Silicone Rubber for Molding and Extrusion

Time:2022-06-09 14:00Writer:djsilicone View:21914

经济型模压胶      经济型挤出胶1

ECONOMIC SILICONE RUBBER FOR MOLDING 


Characteristics:

● Good processability                                                                                                                                        

Main Applications:

● Common silicone rubber products and miscellaneous parts, especially pigmented products.

● Silicone keypads.

Typical Data

Properties

Product Data

Test Method

NE-5140

NE-5150

NE-5160

NE-5170

NE-5180

Appearance

Milk-white, light yellow, light gray,

no obvious extraneous matter.

Visual Inspection

Density, g/cm3

1.101.14

1.131.17

1.161.20

1.191.23

1.201.24

ASTM D792

Hardness, Shore A

40±2

50±2

60±2

70±2

80±2

ASTM D2240

Tensile Strength, MPa, ≥

6.5

7.0

6.5

6.0

ASTM D412

Elongation at Break, %, ≥

420

320

280

200

150

Tension Set, %, ≤

8

6

Tear Strength, Die C, kN/m, ≥

16

18

16

ASTM D624

Compression Set, 180*22h,

40

35

30

ASTM D395

Resilience, %,

60

50

45

/














Physical data in the above table is for reference only.

● Vulcanization condition: 175℃*5Min.

● Ratio of curing agent liquid 2,5-Dimethyl-2,5-di(tert-butylperoxy) hexane: 0.65%.

●The supplied test report is obtained by the Quality Inspection Department with the curing conditions and testing method of the company; due to the difference of curing conditions and testing method, we can’t guarantee that both parties obtain the same testing result, and we suggest that users should use the test data obtained under their own testing conditions as the reference for service performance. All the above performance data and application recommendations are only a reference for use on the service performance of product, instead of a guarantee on the effectiveness or general applicability of our products under a certain application.



ECONOMIC SILICONE RUBBER FOR EXTRUSION 

Characteristics:

● Good processability

Main Applications:

● Low-end miscellaneous extruded silicone rubber products.

Typical Data

Properties

Product Data

Test Method

NE-5240

NE-5250

NE-5260

NE-5270

NE-5280

Appearance

Milk-white, light yellow, light gray,

 no obvious extraneous matter.

Visual Inspection

Density, g/cm3

1.101.14

1.131.17

1.161.20

1.191.23

1.201.24

ASTM D792

Hardness, Shore A

40±2

50±2

60±2

70±2

80±2

ASTM D2240

Tensile Strength, MPa,

6.5

7.0

6.5

6.0

ASTM D412

Elongation at Break, %,

420

320

280

200

150

Tension Set, %,

10

8

Tear Strength, Die C, kN/m,

16

18

16

ASTM D624

Compression Set, 180*22h,

40

35

30

ASTM D395

Resilience, %,

50

45

/


● Physical data in the above table is for reference only.

● Vulcanization condition: 175℃* 5Min.

● Ratio of curing agent liquid 2,5-Dimethyl-2,5-di (tert- butylperoxy) hexane: 0.65%.

●The supplied test report is obtained by the Quality Inspection Department with the curing conditions and testing method of the company; due to the difference of curing conditions and testing method, we can’t guarantee that both parties obtain the same testing result, and we suggest that users should use the test data obtained under their own testing conditions as the reference for service performance. All the above performance data and application recommendations are only a reference for use on the service performance of product, instead of a guarantee on the effectiveness or general applicability of our products under a certain application.




Related material download:

ROHS and Other Restricted Substances Test for Silicone Rubber

Substances of Very High Concern Test(SVHC) for Silicone Rubber

MSDS-Economic Silicone Rubber for Molding and Extrusion

Economic Silicone Rubber for Molding and Extrusion

FDA Test for Silicone Rubber

TSCA-Silicone Rubber

US California Proposition 65-Siliocne Rubber

Perfluoroalkyl and PFAS-Silicone Rubber


 

● Physical data in the above table is for reference only.

● Vulcanization condition: 175*5Min.

● Ratio of curing agent liquid 2,5-Dimethyl-2,5-di(tert-butylperoxy) hexane: 0.65%.

●The supplied test report is obtained by the Quality Inspection Department with the curing conditions and testing method of the company; due to the difference of curing conditions and testing method, we can’t guarantee that both parties obtain the same testing result, and we suggest that users should use the test data obtained under their own testing conditions as the reference for service performance. All the above performance data and application recommendations are only a reference for use on the service performance of product, instead of a guarantee on the effectiveness or general applicability of our products under a certain application.